Corrosion Resistant Alloys

Chemical Composition
Classification | Alloy |
UNS (JIS) |
Nominal Chemical Composition(wt%) | Heat Treatment | Tensile Strength(N/mm²) | Elongation(%) | |||||
Ni | Cr | Mo | Co | Fe | others | ||||||
Corrosion Resistant Alloys | DSALOY200 | N02200 (NW2200) |
≧99.0 | - | - | - | ≦0.4 | C ≦ 0.15 Cu ≦ 0.2 |
A | ≧380 | ≧30 |
DSALOY201 | N02201 (NW2201) |
≧99.0 | - | - | - | ≦0.4 | C ≦ 0.02 Cu ≦ 0.2 |
A | ≧340 | ≧30 | |
DSALOY400 | N04400 (NW4400) |
≧63.0 | - | - | - | ≦2.5 | Cu 28.0-34.0 | A | ≧480 | ≧35 | |
DSALOY K-500 |
N05500 (NW5500) |
bal. | - | - | - | ≦2.0 | Cu 27.0-34.0 Al 2.2-3.2 Ti 0.35-0.85 |
ST+AG | ≧830 | ≧15 | |
DSALOY 600 | N06600 (NCF600) |
≧72.0 | 14.0- 17.0 |
- | - | 6.0- 10.0 |
Cu ≦ 0.50 | A | ≧550 | ≧30 | |
DSA760 | - | bal. | (38) | - | - | - | (Al 3.8) | ST+AG | ≧1,500 | - | |
DSALOY 625 |
N06625 (NCF625) |
≧58.0 | 20.0- 23.0 |
8.0- 10.0 |
≦1.0 | ≦5.0 | Al ≦ 0.40 Ti≦ 0.40 Nb+Ta 3.15-4.15 |
A | ≧760 | ≧30 | |
DSALOY C-276 |
N10276 (NW0276) |
bal. | 14.5- 16.5 |
15.0- 17.0 |
≦2.5 | 4.0- 7.0 |
W 3.0-4.5 V ≦0.35 |
A | ≧690 | ≧40 | |
DSALOY 22 |
N06022 (NW6022) |
bal. | 20.0- 22.5 |
12.5- 14.5 |
≦2.5 | 2.0- 6.0 |
W 2.5-3.5 V ≦0.35 |
A | ≧690 | ≧45 | |
DSALOY CB3 |
N08020 | 32.0- 38.0 |
19.0- 21.0 |
2.0- 3.0 |
- | bal. | Cu3.0-4.0 Nb≦1.0 |
ST | ≧550 | ≧30 | |
DSALOY 25-6MO |
N08925 | 24.0- 26.0 |
19.0- 21.0 |
6.0- 7.0 |
- | bal. | Cu 0.5-1.5 N 0.15-0.25 |
ST | ≧650 | ≧35 | |
DSP5 | S35000 | 4.0- 5.0 |
16.0- 17.0 |
2.5- 3.2 |
- | bal. | Mn 0.5-1.25 | ST+AG | ≧1,300 | ≧4 |
A:Annealing ST:Solution heat Treatment AG:Aging
Features Applications
Classification | Alloy | Features | Applications |
Corrosion Resistant Alloys |
DSALOY 200 |
Good mechanical properties, Excellent corrosion resistance to many corrosive media | Production facilities for foods, caustic soda, chemicals and synthetic fibers, Electrical and electronic components |
DSALOY 201 |
Excellent cold workability, No embrittlement by carbon above 300℃ | Similar applications to DSALOY200, Cold deep-drawn parts | |
DSALOY 400 |
High strength, Good workability, Excellent corrosion resistance to many corrosive environments | Facilities of seawater desalination, salt production and oil refining, Marine construction coverings, Heat exchangers | |
DSALOY K-500 |
Similar corrosion resistance to DSALOY400, Higher strength than DSALOY400, Completely non- magnetic even at -100℃ | Parts requiring higher strength than DSALOY400, Oil-drilling tools, Corrosion resistant valves and springs, Rotary pumpshafts, Fasteners | |
DSALOY 600 |
Good oxidation resistance at high temp. , Corrosion resistance to pure water/alkali/Cl - ion (SCC*) | Equipment for chemical and food production, Heat exchangers, Electronic components | |
DSA760 |
High hardness equivalent to that of martensite stainless steel, High corrosion resistance, Non magnetic | Medical scissors, Dental drills, Automotive turbo parts | |
DSALOY 625 |
High strength without heat treatment, Excellent corrosion resistance in a wide range of severe corrosive environments | Chemical product manufacturing facilities, Aerospace parts, Seawater treatment facilities | |
DSALOY C-276 |
Excellent corrosion resistance in a wide range of severe corrosive environments, Good weldability | Flue-gas desulfurization equipment (FGD), Chemical industrial equipment, Pulp and paper mill facilities | |
DSALOY 22 |
Excellent acid corrosion resistance to many types of corrosion such as SCC, pitting and intergranular corrosion | Chemical manufacturing equipment, Combustion gas FGD, Bleaching equipment at paper mills | |
DSALOY CB3 |
Excellent acid corrosion resistance to many types of corrosion such as pitting, crevice corrosion and intergranular corrosion | Chemical and petrochemical product manufacturing equipment parts (tanks, heat exchangers, piping, pumps, valves) | |
DSALOY 25-6MO |
Corrosion resistance to pitting, crevice corrosion and non-oxidizing acids such as sulfuric acid and phosphoric acid | Tubes for petrochemical industry and seawater cooling equipment, Salt production plant parts, Biochemical equipment parts | |
DSP5 | Similar strength to martensitic stainless steel , Excellent corrosion resistance to non-oxidizing acid | Bellows , Automotive parts , Various sealing parts |
*SCC(Stress Corrosion Cracking)
Specifications・Available Products
Classification | Alloy | Available Products | Specifications | |||
Bar | Wire rod | Strip | ASTM | JIS | ||
Corrosion Resistant Alloys |
DSALOY 200 |
◎ | ◎ | ◎ |
B160 B162 |
G4902 H4553 H4554 |
DSALOY 201 |
◎ | ◎ | ◎ |
B160 B162 |
G4902 H4553 H4554 |
|
DSALOY 400 |
◎ | ◎ | ◎ |
B127 B164 B564 |
G4902 H4553 H4554 |
|
DSALOY K-500 |
○ | - | - | B865 | H4553 | |
DSALOY 600 |
◎ | ◎ | ◎ |
B166 B168 B564 |
G4901 G4902 |
|
DSA760 | ○ | ◎ | - | - | - | |
DSALOY 625 |
◎ | ◎ | ◎ |
B443 B446 B564 |
G4901 G4902 |
|
DSALOY C-276 |
◎ | ◎ | ◎ |
B564 B574 B575 |
G4902 H4553 H4554 |
|
DSALOY 22 |
◎ | ◎ | ◎ |
B564 B574 B575 |
G4902 H4553 H4554 |
|
DSALOY CB3 |
◎ | ◎ | - |
B472 B473 |
- | |
DSALOY 25-6MO |
○ | ◎ | - |
B472 B649 |
- | |
DSP5 | - | - | ◎ | A693 | - |
◎:Standard ◯:Available ー:Not available